Sign In | Join Free | My burrillandco.com
Home > Alloy Round Bar >

14-4PH Alloy Round Bar 14-4PH Superalloy

    Buy cheap 14-4PH Alloy Round Bar 14-4PH Superalloy from wholesalers
     
    Buy cheap 14-4PH Alloy Round Bar 14-4PH Superalloy from wholesalers
    • Buy cheap 14-4PH Alloy Round Bar 14-4PH Superalloy from wholesalers
    • Buy cheap 14-4PH Alloy Round Bar 14-4PH Superalloy from wholesalers

    14-4PH Alloy Round Bar 14-4PH Superalloy

    Ask Lasest Price
    Brand Name : PANGANGGROUP,ANSTEEL,TISCO,BAOSTEEL
    Model Number : 14-4PH
    Certification : SGS,TUV,BV,ISO,MTC
    Price : Negotiations
    Payment Terms : T/T
    Supply Ability : 55000KGS/Month
    Delivery Time : Ex-stock for delivery: 3-7 days Production lead time: 30-60 days
    • Product Details
    • Company Profile

    14-4PH Alloy Round Bar 14-4PH Superalloy

    14-4PH Alloy Round Bar 14-4PH Superalloy


    Description


    14-4PH Alloy Round Bar 14-4PH Superalloy is High temperature alloys and other special alloys

    All of 14-4PH Alloy Round Bar 14-4PH Superalloy conform to Military standard, nuclear power. 100% Ultrasonic test ASTM E2375 /SAE AMS 2154 /SEP 1923 /GB/T 4162 /EN 10228-3.

    • Material:Metal, Alloy Round Bar, 14-4PH
    • Shape:Alloy Round Bar
    • Round bar / Wire rod (Diameter): 5.5mm to 800mm
    • Forging piece: stepped shafts with flanks / discs /tubes /slugs /donuts /cubes /other different shapes based on OEM.
    • Heavy/middle plate via hot rolled: T6 - 200mm X W10 - 1500mm X L1000-12000mm
    • Steel strip via cold rolled: T0.1 - 3mm X W5 - 200mm X L (or in coil form)


    Products Details


    14-4PH Alloy Round Bar 14-4PH Superalloy

    Chemical Composition (weight%):Mechanical Properties Under Final Heat Treatment:
    C(%): 0.03
    Si(%): 0.75
    Mn(%): 0.35
    Cr(%): 14.1
    Ni(%): 4.25
    Mo(%): 2.38
    Co(%): —
    W(%): —
    Al(%): —
    Cu(%): 3.25
    Ti(%): —
    Other(%): Nb 0.25,N 0.02
    TS, σb/≥MPa: 268
    YS, σ0.2≥/MPa: 782
    EL, δ 5≥(%): 13
    Impact, AKV≥/J: 11

    14-4PH Alloy Round Bar 14-4PH Superalloy


    Applications:


    14-4PH Alloy Round Bar 14-4PH Superalloy is often used in the Aerospace, cylinders, gears, hollow shafts, landing gears, marine gas turbine, etc.



    14-4PH Alloy Round Bar 14-4PH Superalloy14-4PH Alloy Round Bar 14-4PH Superalloy


    FAQ


    Q: How do you control the quality?


    A: We have professional inspectors to analyze the chemical composition of raw materials and test the finished products in strict accordance with the standards stipulated in the contract. In this process, the inner and outer surfaces, the appearance of both ends, bending, set length, outer diameter and Wall thickness will be checked one by one. You can rest assured that all products you receive from us are reliable.


    Q: Do you accept customization?


    A: Yes. If you have special requirements for products or packaging, we can make them for you.


    Q: Can you accept trial orders?


    A: Our MOQ is usually 1 ton. However, if you want to place an order as the start of our cooperation, we can accept smaller quantities at the first time. Of course, after the start, we will have further and longer cooperation.


    Q: How do I get samples?


    A: Free samples are available for your inspection and testing, DHL/FedEx/UPS accounts can be used for sampling, and the courier fee is borne by you.


    14-4PH Alloy Round Bar 14-4PH Superalloy

    Quality 14-4PH Alloy Round Bar 14-4PH Superalloy for sale
    Inquiry Cart 0
    Send your message to this supplier
     
    *From:
    *To: Mianyang Baoheng New Material Technology Co.,Ltd
    *Subject:
    *Message:
    Characters Remaining: (0/3000)