Sign In | Join Free | My burrillandco.com
Home > Turbine Blade Steel >

GTD 450 Turbine Blade Steel GTD 450 Superalloy

    Buy cheap GTD 450 Turbine Blade Steel GTD 450 Superalloy from wholesalers
     
    Buy cheap GTD 450 Turbine Blade Steel GTD 450 Superalloy from wholesalers
    • Buy cheap GTD 450 Turbine Blade Steel GTD 450 Superalloy from wholesalers
    • Buy cheap GTD 450 Turbine Blade Steel GTD 450 Superalloy from wholesalers
    • Buy cheap GTD 450 Turbine Blade Steel GTD 450 Superalloy from wholesalers

    GTD 450 Turbine Blade Steel GTD 450 Superalloy

    Ask Lasest Price
    Brand Name : PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL
    Model Number : GTD 450
    Certification : SGS, TUV, BV, ISO, MTC
    Price : Negotiations
    Payment Terms : T/T
    Supply Ability : 45000KGS/Month
    Delivery Time : Ex-stock for delivery: 3-7 days Production lead time: 30-60 days
    • Product Details
    • Company Profile

    GTD 450 Turbine Blade Steel GTD 450 Superalloy

    GTD 450 Turbine blade steel GTD 450 Superalloy


    Size Range



    Round bar / Wire rod (Diameter):5.0mm to 800mm
    Square bar / Flat bar:4.0mm to 1100mm
    Forging piece:

    Stepped shafts with flanks / discs /tubes
    /slugs /donuts /cubes /other different shapes based on OEM.

    Heavy/middle plate via hot rolled:T6 - 350mm X W10 - 1500mm X L1100-13000mm

    Sheet steel via cold rolled:

    T0.5 - 4mm X W6 - 1000mm X L1000 - 1200mm

    Steel strip via cold rolled:

    T0.1 - 5.0mm X W5 - 190mm X L (or in coil form)
    LengthFixed length or random length or based on the customer's special requirement.


    Chemical Composition and standard



    Grade

    GTD 450

    standard--
    Chemical Composition (weight%)
    C (%): 0.03 ~ 0.05 V (%): ≤ 0.10
    Si (%): 0.20 ~ 0.50 N (%): ≤ 0.030
    Mn (%): 0.30 ~ 0.80 Al (%): ≤ 0.030
    P (%)≤: 0.020 Ag (%): ≤ 0.005
    S (%)≤: 0.005 Pb(%): ≤ 0.005
    Cr (%): 14.0 ~ 16.0 Sn(%): ≤ 0.10
    Ni (%): 6.20 ~ 6.80
    Mo (%): 0.60 ~ 1.00
    Cu (%): 1.35 ~ 1.75
    Nb (%): 8 X C ~ 15 X C


    GTD 450 Turbine Blade Steel GTD 450 Superalloy


    Mechanical Properties



    GTD 450 Turbine Blade Steel Mechanical Properties

    Tensile strength,Rm/MPa:1010~1220
    Yield strength,Rp/MPa:≥917
    Elongation/%:≥15
    Reduction of area, ψ/%:≥50
    Impact, KV /J:68
    Annealed hardness HBS:302~363

    Contact us


    If you are interested in our products or have any questions, please contact our team of engineers sales@ss-bars.com

    GTD 450 Turbine Blade Steel GTD 450 SuperalloyGTD 450 Turbine Blade Steel GTD 450 Superalloy





    GTD 450 Turbine Blade Steel GTD 450 Superalloy

    Quality GTD 450 Turbine Blade Steel GTD 450 Superalloy for sale
    Inquiry Cart 0
    Send your message to this supplier
     
    *From:
    *To: Mianyang Baoheng New Material Technology Co.,Ltd
    *Subject:
    *Message:
    Characters Remaining: (0/3000)