    AMS 5674 Superalloy Flat Bar

    Ask Lasest Price
    Brand Name : PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL
    Model Number : AMS 5674
    Certification : SGS, TUV, BV, ISO, MTC
    Price : Negotiations
    Payment Terms : T/T
    Supply Ability : 50000KGS/Month
    Delivery Time : Ex-stock for delivery: 3-7 days Production lead time: 30-60 days
    • Product Details
    • Company Profile

    AMS 5674 Superalloy Flat Bar

    AMS 5674 Superalloy Flat Bar


    Product Information


    AMS 5674 is a high-temperature alloy steel with excellent corrosion resistance and high-temperature performance. It is an alloy of molybdenum, cobalt, chromium, and nickel, commonly used for manufacturing parts that work under high temperature stress, such as blades in turbine engines and blades and rotors in gas turbines. AMS 5674 alloy has good mechanical properties and high-temperature stability, and can be used at temperatures up to 980 ° C. In addition, the alloy has excellent corrosion resistance and can resist corrosion and oxidation in extreme environments.


    Size Range

    Round bar / Wire rod (Diameter):1.0 mm to 1000 mm
    Square bar / Flat bar: 1.0 mm to 1000 mm
    Forging piece: Stepped shafts with flanks / discs /tubes /slugs /donuts /cubes /other different shapes based on OEM.
    Heavy/middle plate via hot rolled: T5.0 - 1000 mm X W3 - 1000 mm X L100-1000 mm
    Sheet steel via cold rolled: T1.0 - 10 mm X W1 - 1000 mm X L100 - 800 mm
    Steel strip via cold rolled: T3.0 - 10 mm X W1.0 - 1000 mm X L (or in coil form)
    Length: Fixed length or random length or based on the customer's special requirement.


    Chemical Composition and standard

    AMS 5674D

    Mechanical Properties

    SAE AMS 5674D

    C(%): ≤0.08
    Si(%): ≤1.00
    Mn(%): ≤2.00
    P(%): 0.035
    S(%)≤: 0.03

    Cr(%): 17.0~19.0
    Ni(%): 9.00~12.0
    Mo(%): ≤0.75
    Nb(%): 10xC~1.10

    Ta(%): ≤0.05

    Cu(%): ≤0.50

    Fe: Remainder


    Tensile strength,Rm/MPa: -
    Yield strength,Rp/MPa: -

    Elongation, A/%: -

    Reduction of area, ψ/%: -

    Hardness HRC: -



    AMS 5674 Superalloy Flat Bar

    Applications

    AMS 5674 is typically used to manufacture parts that operate under high temperature stress, such as blades in turbine engines and blades and rotors in gas turbines.


    If you are interested in our products or have any questions, please contact our team of engineers at
    sales@ss-bars.com


    AMS 5674 Superalloy Flat BarAMS 5674 Superalloy Flat Bar


    AMS 5674 Superalloy Flat Bar

    Quality AMS 5674 Superalloy Flat Bar for sale
    Inquiry Cart 0
    Send your message to this supplier
     
    *From:
    *To: Mianyang Baoheng New Material Technology Co.,Ltd
    *Subject:
    *Message:
    Characters Remaining: (0/3000)